Laserfiche WebLink
2.0 RESULTS <br /> Shredded Greenwaste <br /> The sloped test plot was constructed first, with placement and measurement <br /> proceeding smoothly according to plan. The test plot layout is shown on Figure 1 <br /> and the results are as follows: <br /> Average thickness: 1.02' <br /> Area of plot: 2,500 square feet <br /> Volume of material: 2,550 cubic feet <br /> Weight of material: 68,100 pounds <br /> Density of material: 26.71 pounds/cubic foot or 721.1 pounds/cubic yard <br /> The first level deck test plot for shredded greenwaste was constructed adjacent to <br /> an area previously covered with soil. In the course of material placement, the <br /> northern edge of the test plot was inadvertently blended into the adjacent soil, <br /> causing the edge of the plot to be lost. After unsuccessful attempts to measure the <br /> additional area covered by the weighed material, all parties agreed that this test plot <br /> should be abandoned and re-constructed. The layout of this failed test plot is <br /> presented in Figure 2. <br /> The second level deck test plot constructed for shredded greenwaste proceeded <br /> smoothly. The layout for this test plot is presented in Figure 3, and the results are as <br /> follows: <br /> Average thickness: 1.26' <br /> Area of plot: 2,500 square feet <br /> Volume of material: 3,150 cubic feet <br /> Weight of material: 97,000 pounds <br /> Density of material: 30.79 pounds/cubic foot or 831.4 pounds/cubic yard <br /> 2-1 <br /> J.\Allied\Forward\2006.0154 ADC Test\ADC Test Report\Draft Final ADC Test Report Sec 2.doc <br />