u <br />Precision-• Laboratories <br />MATERIAL DESCRIPTION: 60 Mil HDPE Microspike Geomembrane <br />SAMPLED BY: PGL @ Agru, NV <br />DATE RECEIVED: August 13, 2008 <br />SAMPLE IDENTIFICATIONS: <br />SAMPLE ID <br />R#932681.08 L#8180479 <br />R#932692.08 L#8180479 <br />TESTS REQUIRED: <br />TEST METHOD <br />DATE REPORTED: August 15, 2008 <br />49678 <br />Density <br />Carbon Content <br />Carbon Black Dispersion <br />Core Thickness <br />Tensile Strength <br />Asperity Height <br />TEST CONDITIONS: These samples were conditioned for a minimum one hour in the <br />laboratory at 22 + 2°C (71.6 + 3.6°F) and at 60 + 10% relative humidity prior to test. <br />TEST RESULTS: <br />The test results are summarized in Tables 1 to 2. The units in which the data are reported are <br />included on these tables. <br />DATE: 8/15/2008 <br />Carmelo V. Zantua <br />Technical/Lab Director <br />1160 North Gilbert Street, Anaheim, CA. 92801, Tel# 714-520-9631, Fax# 714-520-9637 <br />