File MH29667 Page TS-2 of 2 issued: 2005-oy-0a <br /> SIMULATED USE RESISTANCE TO FLUIDS TEST (FIBERGLASS REINFORCED PLASTIC SUMP <br /> MATERIALS) : <br /> METHOD <br /> One sample assembly as described in Item B was placed in a container <br /> filled with each of the Fluids Listed below such that the fittings inside the <br /> container were completely covered with the fluids. The samples and fluids <br /> were maintained at a temperature of 100°F throughout the exposure. Following <br /> 30 days in this condition, the containers were subjected to an internal <br /> pressure of 4.5 psig (based on a maximum sump depth of 10.3 ft.) for a period <br /> of at least 5 min. while the samples were examined for evidence of leakage. <br /> 1003 Methanol <br /> 503 Methanol/503 ASTM Reference Fuel C <br /> 154 Ethanol/853 ASTM Reference Fuel C <br /> 103 Ethanol/903 ASTM Reference Fuel C <br /> 153 MTBE/853 ASTM Reference Fuel C <br /> RESULTS <br /> There was no evidence of leakage <br /> SIMULATED USE RESISTANCE TO FLUIDS TEST (FIBERGLASS REINFORCED PLASTIC SUMP <br /> MATERIALS) : <br /> METHOD <br /> One sample assembly as described in Item C was placed in a container <br /> filled with each of the fluids Listed below such that the fittings inside the <br /> container were completely covered with the fluids. The samples and fluids <br /> were maintained at a -temperatureof 100°F throughout the exposure. Following <br /> 30 days in this condition, the containers were subjected to an internal <br /> pressure of 4.5 prig (based on a maximum sump depth of 10.3 ft.) for a period <br /> of at least 5 min. while the samples were examined for evidence of leakage. <br /> 1004 Methanol. ...-__ _.. _. <br /> -503 Methafiol/50V=ASTM-Refnzencd—Fuel C -- - - - -� <br /> 1003 Ethanol - - - <br /> ._._..:503-ECha=I/508=.-ASTM-.-Reif ence-Fuel-C. <br /> 153 Ethanol/858 ASTM Reference Fuel C - <br /> _ <br /> 154 MTBE/858 ASTM Reference Fuel C <br /> RESULTS <br /> There was'iso'evidence of leakage <br />