Laserfiche WebLink
2.0 RESULTS <br /> Shredded Greenwaste <br /> The sloped area test plot (Test Plot #1) was constructed first (10/11/06), with <br /> placement and measurement proceeding smoothly according to plan. The test plot <br /> layout is shown on Figure 1 and the results are as follows: <br /> Average thickness: 1.02' <br /> Area of plot: 2,500 square feet <br /> Volume of material: 2,550 cubic feet <br /> Weight of material: 68,100 pounds <br /> Density of material: 26.71 pounds/cubic foot or 721.1 pounds/cubic yard <br /> Construction of the level deck area test plot for shredded greenwaste (Test Plot#5) <br /> was completed without incident on 10/12/06. The layout for this test plot is <br /> presented in Figure 2, and the results are as follows: <br /> Average thickness: 1.26' <br /> Area of plot: 2,500 square feet <br /> Volume of material: 3,150 cubic feet <br /> Weight of material: 97,000 pounds <br /> Density of material: 30.79 pounds/cubic foot or 831.4 pounds/cubic yard <br /> A sample of shredded greenwaste was collected from the stockpile on October 12, <br /> and was subsequently tested for moisture content at a compost laboratory. <br /> Overall density for shredded greenwaste as tested in this program (Test Plots #1 and <br /> #5) are: 28.75 pounds/cubic foot or 776.3 pounds/cubic yard. <br /> 2-1 <br /> J:\Allied\Forward\2006.0154 ADC Test\ADC Test Report\Final ADC Test Report Sec 2.doc <br />