Tank#16 was patched usinfke Epoxy and Fiber Glass Mat methoo coat of Epoxy was applied <br /> to the area of the holes larger than the mat dimensions . The Fiber Glass Mat was pressed in to the <br /> first coat of Epoxy directly after the first coat was applied.A second coat of Epoxy was applied over <br /> the Fiber Glass Mat and overlapped up the sides of the tank. This patch was allowed to cure before <br /> the final lining was applied to the inside of the tank. <br /> EPDXY LINING <br /> The Epoxy lining was applied by the spray method. This author reviewed the Contractors lining <br /> methods of mixing and application of the Epoxy lining and found them to meet the requirements of <br /> the San Joaquin County Environmental Health Department(ED)letter of January 5,2011,under <br /> the hand of Kasey Foley, program director, and the standards of the industry. After the lining was <br /> cured,this author inspected the lining and found that it met the above stated requirements. <br /> COMPLETION <br /> The lining was tested by the prescribed method in the ED letter and is ready for final leak testing. <br /> After testing the tanks may be returned to service as a Underground Storage Tank. <br /> Any questions on this report should be directed to the under signed at(209)368-9381. <br /> Respectfully submitted, <br /> Foothill Engine* v�o -sif <br /> "IF <br /> trvin R e urg, <br /> sT I V I <br /> %N,41 <br /> OF <br /> 2 <br />