Laserfiche WebLink
Lay out fiberglass materials at each seam to be bonded. (2 x 1.5oz.FRP matt for collar attachment. <br /> 2 x 1.5 oz. and 1 x 18 oz.woven roving material for direct attachment.) <br /> ALWAYS WEAR GLOVES WHEN HANDLING FIBERGLASS BONDING MATERIALS. <br /> Wet-out or soak,with brush,liquid resin over fiberglass cloth material completely,material will go <br /> clear when fully saturated. Use pig bristle roller tool to"roll-out"air bubbles gently,so as not to <br /> displace putty.Remove all bubbles. Apply additional layers of material in same manner.Your <br /> laminate should appear clear,with no air bubbles or pockets in view and all fasteners covered. If <br /> additional resin is required,-use only resin from Western Fiberglass, Inc. The resin used in <br /> construction of all Western Fiberglass, Inc. components is corrosion resistant resin,made for use in <br /> fuel and chemical applications. <br /> TEST PROCEDURES <br /> After the sump to tank fitting is completed,you shall test the integrity of your seal. This is <br /> important to,insure that the sump riser tube/tank bond will not allow any contained.fluid to leak. <br /> Check with local regulations for required testing procedures.A common test procedure is to fill the <br /> sump with water after the sump/tank bond has completely cured,usually overnight,and observe <br /> bond seam for any leaks. NOTE: U.L.Listed sumps require a listed,approved,electronic <br /> monitor/alarm system to be installed for operator notification in the event of prod"nct leakage <br /> within sump area. <br />